    QI Cheng-lin, ZHANG Jian-liang, LIN Zhong-chun, YIN Jian, CHANG Jian, LU Wei-jia. Erosion of carbon bricks at the hearth sidewall by harmful elements in a blast furnace[J]. Chinese Journal of Engineering, 2011, 33(4): 491-498. doi: 10.13374/j.issn1001-053x.2011.04.019
    Citation: QI Cheng-lin, ZHANG Jian-liang, LIN Zhong-chun, YIN Jian, CHANG Jian, LU Wei-jia. Erosion of carbon bricks at the hearth sidewall by harmful elements in a blast furnace[J]. Chinese Journal of Engineering, 2011, 33(4): 491-498. doi: 10.13374/j.issn1001-053x.2011.04.019

    Erosion of carbon bricks at the hearth sidewall by harmful elements in a blast furnace

    doi: 10.13374/j.issn1001-053x.2011.04.019
    • Received Date: 2010-05-17
      Available Online: 2021-07-30
    • Publish Date: 2021-07-30
    • Seven samples of a blast furnace at representative positions were analyzed by scanning electron microscopy(SEM),energy dispersive spectrometry(EDS),X-ray diffraction(XRD) and atomic absorption spectrometry to study the erosion of carbon bricks at the BF hearth sidewall by harmful elements and the mechanism of pulverizing fracture.The results show that the erosion mechanism of carbon bricks at different parts of the hearth is different.In the first layer the erosion is mainly caused by the catalytic effects of harmful elements in the carbon loss reaction and the generation of leucite;in the upper area,penetration of K into brick work joints leading to a quality change of carbon bricks plays the leading role;in the tuyere,Zn is the main cause of erosion;but in the taphole the content of K is larger,with enrichment of Pb.It is also found that a harmful element has different effects at different parts of the hearth.In the upper area,the erosion mechanism is mainly the catalytic effect of K in the erosion reaction,but in lower part is the penetration of K into carbon bricks leading to a quality change of carbon bricks;Zn significantly crystallizes on carbon bricks in the tuyere,however in the hearth bottom Zn attaches to carbon bricks without obvious crystallization.

       

    • loading
    • 加載中

    Catalog

      通訊作者: 陳斌, bchen63@163.com
      • 1. 

        沈陽化工大學材料科學與工程學院 沈陽 110142

      1. 本站搜索
      2. 百度學術搜索
      3. 萬方數據庫搜索
      4. CNKI搜索
      Article views (279) PDF downloads(10) Cited by()
      Proportional views
      Related

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return
      中文字幕在线观看