    WANG Min, BAO Yan-ping, YANG Quan. Effect of ferro-titanium alloying process on steel cleanness[J]. Chinese Journal of Engineering, 2013, 35(6): 725-732. doi: 10.13374/j.issn1001-053x.2013.06.016
    Citation: WANG Min, BAO Yan-ping, YANG Quan. Effect of ferro-titanium alloying process on steel cleanness[J]. Chinese Journal of Engineering, 2013, 35(6): 725-732. doi: 10.13374/j.issn1001-053x.2013.06.016

    Effect of ferro-titanium alloying process on steel cleanness

    doi: 10.13374/j.issn1001-053x.2013.06.016
    • Received Date: 2012-03-05
    • The main factors were studied which influence the titanium yield during a ferro-titanium alloying process. The inclusion phases and removal effect were comparatively analyzed before and after ferro-titanium alloying. When controlling the activity of oxygen (a[o]) before deoxidation below 350×10-6, the interval time between Al and Ti addition above 3 min can guarantee the titanium yield above 85%. With a[o] above 350×10-6, the interval time between Al and Ti addition should be extended more than 5 min. Extending the interval time between Al and Ti addition can improve the titanium yield at the same a[o] and [Al]s. During RH refining, Al2O3 inclusions with the equivalent diameter above 200 μm can float and be removed within 5 min, but the removal time of AI-Ti-O inclusions with the same size is 1 to 2 min more than pure Al2O3. Al-Ti-O complex inclusions form around Al2O3 after the titanium alloy being added into the melt, and the titanium yield decreases due to the formation of these inclusions.

       

    • loading
    • 加載中

    Catalog

      通訊作者: 陳斌, bchen63@163.com
      • 1. 

        沈陽化工大學材料科學與工程學院 沈陽 110142

      1. 本站搜索
      2. 百度學術搜索
      3. 萬方數據庫搜索
      4. CNKI搜索
      Article views (225) PDF downloads(16) Cited by()
      Proportional views
      Related

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return
      中文字幕在线观看