    DENG Xiao-xuan, WANG Xin-hua, LI Lin-ping, WEI Peng-yuan, JI Chen-xi, CENG Zhi, TIAN Zhi-hong. Effect of ladle change process on the surface cleanliness of IF steel continuous casting slabs[J]. Chinese Journal of Engineering, 2014, 36(7): 880-886. doi: 10.13374/j.issn1001-053x.2014.07.005
    Citation: DENG Xiao-xuan, WANG Xin-hua, LI Lin-ping, WEI Peng-yuan, JI Chen-xi, CENG Zhi, TIAN Zhi-hong. Effect of ladle change process on the surface cleanliness of IF steel continuous casting slabs[J]. Chinese Journal of Engineering, 2014, 36(7): 880-886. doi: 10.13374/j.issn1001-053x.2014.07.005

    Effect of ladle change process on the surface cleanliness of IF steel continuous casting slabs

    doi: 10.13374/j.issn1001-053x.2014.07.005
    • Received Date: 2013-05-05
      Available Online: 2021-07-19
    • The effect of ladle change process (the 4th heat to the 5th heat) on the surface cleanliness of IF steel continuous casting slabs was investigated by total oxygen measurement and automatic feature analysis equipped on ASPEX. A comparison of surface cleanliness was performed between transition slabs (cast during ladle change process) and normal slabs (cast under normal condition). It is found that inclusions larger than 20μm are classified into three types:(1) cluster alumina (including bubble + cluster alumina inclusions);(2) cluster TiOx-Al2O3 inclusions; and (3) mold powder inclusions. In terms of surface inclusions in normal slabs, most of the inclusions detected in the scanning area are cluster alumina, and no mold powder inclusions are found. While for transition slabs, the total oxygen content increases from 14×10-6 to 17×10-6, and the number density of Type 2 inclusions goes up since the cast start of the 5th heat, indicating re-oxidation of the steel melt during ladle change process. Furthermore, level fluctuation in the mold is also severe since the cast start of the 5th heat, leading to mold powder entrapments. The affected length of cast slabs during ladle change process is about 11 m under the present casting condition.

       

    • loading
    • 加載中

    Catalog

      通訊作者: 陳斌, bchen63@163.com
      • 1. 

        沈陽化工大學材料科學與工程學院 沈陽 110142

      1. 本站搜索
      2. 百度學術搜索
      3. 萬方數據庫搜索
      4. CNKI搜索
      Article views (307) PDF downloads(11) Cited by()
      Proportional views
      Related

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return
      中文字幕在线观看